L605 Cobalt Based High-temperature Alloy Haynes 25 Rods

1
L605 Chemical Compositions


C:0.05~0.15
Cr:19.0~21.0
Ni:9.0~11.0
W:14.0~16.0
Co: margin
Mn:1.0~2.0
Fe:≤3.0
Si:≤0.40
P:≤0.04
S:≤0.03

 

2
Physical Properties

 

Density ρ=9.13g/cm3

L605 cobalt-based superalloy Haynes 25 round rod can be customized

L605, also known as HAYNES25, is a cobalt-based alloy with good formability and high-temperature properties. In high-temperature and high-strength environments, the material can resist oxidation, carbonization, and is not easy to crack. L605 HAYNES®25, UNS R30605, AMS5759F, AMS5537, ASTM F90, AMS 5796

L605 cobalt-based alloy

L605 is a cobalt-based alloy with good formability and excellent high temperature properties. At 1800°F, L605 has a 7000psi, 100-hour stress cracking strength. At 1900°F, L605 is still resistant to oxidation and carburization Ability. The delivery state of heat treatment solution treated L605 is mostly in solid solution state with excellent performance. The material's solution temperature range is 2150-2250°F, and then quickly air cooled or water quenched. Thin sheets with a thickness of less than 0.025" Solution temperature is 2150°F, then rapid air cooling or water quenching; sheet thickness 0.026" and above is solution temperature 2200°F, then rapid air cooling or water quenching; thick plate solution temperature is 2200°F, then water quenching ;The solid solution temperature of the bar is 2250°F, and then water quenched. Cold working and aging improve the performance of the material at room temperature and heated environments. Proper cold working and aging treatment can provide the tensile strength of the material at room temperature and heated environments. Strength. Moderate cold work can increase creep strength to 1800°F and stress crack strength to 1500°F. Aging temperatures range from 700-1100°F. Aging has little effect, but Improves creep and crack strength of materials below 1300°F.

3
Processing Performance


Haynes 25 can be processed by conventional processes. It is recommended to use cobalt-containing high-speed steel or alloy steel cutting tools. Compared with austenitic stainless steel (such as 304, 321, 347 stainless steel), Haynes 25 is more difficult to process. The high cold work hardening rate and the large amount of heat generated during processing make processing very difficult. It is recommended to use small feed amount and low speed.

Welding
L605 can be welded by shielded metal arc welding, gas tungsten arc welding, and gas metal arc welding. Submerged arc welding is not recommended.

Before welding, the welding surface needs to be thoroughly cleaned, wipe off any stains and dry the surface.

 

4
Applications


L605 is mostly used in the manufacture of jet engine components, including engine blades, combustion chambers, reburning devices, and turbine rings. L605 is also used in industrial furnaces, including flame barriers and linings in key parts of high-temperature furnaces.

 

5
Corrosion Resistance


L605 has demonstrated excellent resistance to high-temperature corrosive gases in jet engine applications. The oxidation resistance of intermittent operation at 1600°F and continuous operation at 2000° is also very good. During the heating process, L605 is highly resistant to oxidation and no material will appear. Peeling. At the same time, the material is resistant to a variety of chemical oxidants, especially hydrochloric acid and nitric acid at a certain concentration and temperature. It has good resistance to salt spray corrosion.

Haynes 25 MATERIAL

Learn More

Send Inquiry